You can do an ionic test. Chrysler and GM, I know for sure have their
own specs for ionics in regards to under hood boxes where the control
circuits are housed.
In regards to "invisible crud" perhaps a Millipore test (Gravimetric
particle) could at least confirm the effectiveness of the solvent in
removing chips and other metal fines.
Charlie
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Thursday, June 10, 2004 9:06 AM
To: [log in to unmask]
Subject: [TN] Cleaning fluid and ionic contamination
Good morning Technetters,
We now have a Safety-Kleen system which is being used for cleaning some
parts that ultimately go into dielectric oil in a high voltage system.
The solvent used is "Safety-Kleen Premium Solvent" which is basically
Naphtha. The system filters and re-distills the solvent to keep it
"clean".
My question is, once a part has been washed and dried, just how clean is
it? It may be grease free, but how much invisible crud may be lurking
on the part that once installed into a high voltage system can cause
high voltage breakdown either short term or long term?
How can we profile the relative cleanliness of the parts?
Thanks in advance for your guidance.
Phil Nutting
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|