TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Fri, 27 May 2005 09:45:15 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (77 lines)
Brian,
You wrote:
"Edge-dip tests, such as I described, done under
scientifically regulated and repeatable conditions, do yield wetting
speed data and they show dewetting better than any other method."

1) Sounds like a wetting balance to me!
2) How can it be better than a wetting balance if it doesn't give
numerical results?

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: May 27, 2005 9:41 AM
To: [log in to unmask]
Subject: Re: [TN] Wetting balance

Gerard O'Brien wrote:
>         2.dip and look tests do not yield wetting speed data, impact
of
> temperature on wetting speed/force, show de-wetting ( Brian E - I have
> unfortunately many thousand curves showing dewetting which upon
further
> analysis was confirmed as poor basis metal pre-treatment)

Whereas I agree with you that dewetting is most often caused by poor
preparation of the base metal (usually either the presence of organics,
such as bleed-through and/or the use of abrasives), I don't understand
your other contentions. Edge-dip tests, such as I described, done under
scientifically regulated and repeatable conditions, do yield wetting
speed data and they show dewetting better than any other method. If you
change the solder bath temp, you could also determine the effect on
wetting speed. Maybe you are confusing what I was describing with the
IPC edge-dip test with the cam-driven arm, which had a dwell time (4
sec, if I remember correctly) that would be useless for wetting time
determination although excellent for dewetting.

In the 1960s, I did about three years (intermittent) research into the
causes and cures for dewetting, as this was a real pest at that time.

Brian

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2