TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 6 May 2005 08:39:23 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
      Hi Brian:
                    My apologies I was not specific enough. I need to know of flux products that are water soluble *>>>>>>low to mild activated<<<<* that are working well through reflow and wave solder. In other words I need some testimonials about specific products. All the flux manufacturer guidelines need to be followed and will be followed. Thanks for all inputs.
        Regards,
        Ramon
        	

-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Friday, May 06, 2005 2:36 AM
To: TechNet E-Mail Forum; Dehoyos, Ramon
Subject: Re: [TN] Flux


The first point that should be made is that ALL fluxes used in
electronics assembly are organic, from the mildest pure water-white
rosin, via all the "no-clean" varieties to the most active water-soluble
flux. The only inorganic fluxes for soft soldering commonly used for
non-electronics purposes are the zinc chloride/ammonium
chloride/hydrochloric acid mixtures plus a few speciality fluxes for
specific purposes on "difficult" metals.

This makes your question rather vague, especially as you mentioned 
"cleaned" without specifying which method you use. If, for example, you 
use just water, then any flux that is not water-soluble would obviously 
be unsuitable (and, possibly, some that are!).

If the board has been successfully cleaned, then RMA or any other flux 
type may be used for repair, as you are not mixing residues. You will 
have to decide whether it needs to be cleaned or not. In most cases, 
especially with hand soldering, it would be safe not to clean after RMA, 
but the results may look unsightly.

Brian

Dehoyos, Ramon wrote:
> All Technetters: What are some of the Organic fluxes mild to low
> activation that are out there and have been proven to work on surface
> mount components in paste and wave solder machine? Also after a board
> has been built using organic flux and cleaned, gone out to customers
> and returned to be repaired, is it safe to use RMA flux? My
> understanding has been that it is not recommended. Thanks in advance.
>  Ramon
> 
> --------------------------------------------------- Technet Mail List
> provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send
> a message to [log in to unmask] with following text in the BODY (NOT
> the subject field): SIGNOFF Technet To temporarily halt or (re-start)
> delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815 
> -----------------------------------------------------
> 

-- 
______________________________________________
Please note new e-mail address [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2