TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 6 May 2009 12:58:08 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="UTF-8"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Rock on...
 
 
In a message dated 5/6/2009 9:46:20 A.M. Pacific Daylight Time,  
[log in to unmask] writes:

My  motives aren't but my façade is, so I'll pass.
Dewey

-----Original  Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham  Naisbitt
Sent: Wednesday, May 06, 2009 9:36 AM
To:  [log in to unmask]
Subject: Re: [TN] What does HIGH GRADE FR-4  mean?

Stone me!

Graham Naisbitt

On 6 May 2009, at 14:51,  Douglas Pauls wrote:

> I would say that Dewey has lost his  marble.......
>
> Doug Pauls
> Rockwell  Collins
>
>
>
> "Whittaker, Dewey (EHCOE)"  <[log in to unmask]>
> Sent by: TechNet  <[log in to unmask]>
> 05/06/2009 08:48 AM
> Please respond  to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond  to
> "Whittaker, Dewey (EHCOE)"  <[log in to unmask]>
>
>
> To
>  [log in to unmask]
> cc
>
> Subject
> Re: [TN] What does  HIGH GRADE FR-4 mean?
>
>
>
>
>
>
>  It is. I thought you'd just take the rest for granite.
>  Dewey
>
> -----Original Message-----
> From: Inge  [mailto:[log in to unmask]]
> Sent: Tuesday, May 05, 2009 11:24  PM
> To: TechNet E-Mail Forum; Whittaker, Dewey (EHCOE)
> Subject:  Re: [TN] What does HIGH GRADE FR-4 mean?
>
> only seven  shall's...is the stone plate complete? Nothing about  
>  dielectric
>
> constant which I count as a primary  requirement..and copper
> adhesion...and...?
>  Inge
>
>
> ----- Original Message -----
> From:  "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
> To:  <[log in to unmask]>
> Sent: Tuesday, May 05, 2009 8:53 PM
>  Subject: Re: [TN] What does HIGH GRADE FR-4 mean?
>
>
>  Since Ken and Doug have attempted to handle the humor, I guess I'll   
> have
> to
> fill in the technical details. A list of  requirements is as follows:
>
>
>
> *     The laminate shall have maximum moisture absorption  of  
> 0.5% (The
>
> actual fabricated bare PB shall  have 0.2 % prior to processing).
>
> *       The laminates and bonding materials shall have a  
>  flammability
> rating of V-0 minimum.
>
> *     The laminate shall have a glass transition temperature  of  
> 170°C
> minimum.
>
> *       The laminate shall have a decomposition temperature of  340°C
> minimum.
>
> *         The  allowable point to point variation of the laminate Z- 
> Axis
>  CTE
> shall be no greater than 3.5% (ideally 3.0% or less) when  tested  
> between
> 50
> to 260°C.
>
>  *         The laminate shall demonstrate meeting the  requirements for
> thermal resistance to T288 testing for a minimum of 5  minutes.
>
> *         There shall be  objective evidence that the laminate  
> material is
>  resistant to conductive anodic filament (CAF)  growth.
>
>
>
> There are other things to consider  such as phenolic cure systems and
> plating
> adhesion, but this  is a start. IPC-4101/126 and /129 are good  
> examples of
>  high performance FR4s.
>
> Dewey
>
>
>
>  -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On  Behalf Of Harris Dy
> Sent: Tuesday, May 05, 2009 10:23 AM
> To:  [log in to unmask]
> Subject: [TN] What does HIGH GRADE FR-4  mean?
>
>
>
> Hi All,
>
>
>
>  Can anyone define High Grade FR-4?
>
>
>
> I think  it's a vague requirement that I see on customer drawing. Is  
>  this
> something that should be obsolete now because today customer  should  
> really
>
> provide the properties of the  laminate that they want to use... eg  
> Tg, Td,
>
>  Dk.
>
>
>
> Can anyone shed some  light?
>
>
>
> Thanks,
>
>  Harris
>
>
>
>
>
>
>
>
>
>  ---------------------------------------------------
>
> Technet  Mail List provided as a service by IPC using LISTSERV 15.0
>
> To  unsubscribe, send a message to [log in to unmask] with following  
>  text in
>
> the BODY (NOT the subject field): SIGNOFF  Technet
>
> To temporarily halt or (re-start) delivery of Technet  send e-mail to
> [log in to unmask]: SET Technet NOMAIL or  (MAIL)
>
> To receive ONE mailing per day of all the posts: send  e-mail to
> [log in to unmask]: SET Technet Digest
>
> Search  the archives of previous posts at:  
http://listserv.ipc.org/archives
>
> Please visit IPC web site  
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
> for  additional information, or contact Keach Sasamori at [log in to unmask]  
>  or
>
> 847-615-7100 ext.2815
>
>  -----------------------------------------------------
>
>
>
>
>  ---------------------------------------------------
> Technet Mail List  provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send  a message to [log in to unmask] with following  
> text in
>  the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt  or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET  Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the  posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>  Search the archives of previous posts at:  
http://listserv.ipc.org/archives
> Please visit IPC web site  
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
> for  additional information, or contact Keach Sasamori at [log in to unmask]  
>  or
>
> 847-615-7100 ext.2815
>  -----------------------------------------------------
>
>  ---------------------------------------------------
> Technet Mail List  provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send  a message to [log in to unmask] with following  
> text in
>  the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt  or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET  Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the  posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>  Search the archives of previous posts at:  
http://listserv.ipc.org/archives
> Please visit IPC web site  
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional  information, or contact Keach Sasamori at [log in to unmask] 
>   or
> 847-615-7100 ext.2815
>  -----------------------------------------------------
>
>
>  ---------------------------------------------------
> Technet Mail List  provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send  a message to [log in to unmask] with following  
> text in
>  the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt  or (re-start) delivery of Technet send e-mail to 
[log in to unmask] 
> :  SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the  posts: send e-mail to 
[log in to unmask] 
> : SET Technet Digest
>  Search the archives of previous posts at:  
http://listserv.ipc.org/archives
> Please visit IPC web site  
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
>  for additional  information, or contact Keach Sasamori at [log in to unmask] 
>  or  847-615-7100 ext.2815
>  -----------------------------------------------------

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

**************Big savings on Dell’s most popular laptops. Now starting at 
$449! 
(http://pr.atwola.com/promoclk/100126575x1221827510x1201399090/aol?redir=http:%2F%2Fad.doubleclick.net%2Fclk%3B214663377%3B36502382%3Bh)

ATOM RSS1 RSS2