TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 20 Sep 2005 07:51:35 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard" <[log in to unmask]>
Parts/Attachments:
text/plain (19 lines)
Hi, folks
I have a pwb fab drawing that calls out fused tin-lead plating or solder
coating. I know that the solder coating is HASL, but what is fused
tin/lead? My understanding is that it is a tin/lead coating that is
applied to the bare pwb using a reflow oven process. Does this provide a
flat surface of tin/lead? If my only choice of finish is tin/lead, which
process is better in terms of flatness and solderability? I have a
fine-pitch BGA that is going to be assembled on this pwb.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2