TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Barmuta, Mike" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 28 Feb 2001 15:29:52 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
Hi John: Everything stayed in the Electrovert pot here but it did look a
little like a lava lamp on steroids. Other than a couple of boards
submarining into the solderpot all is well.
Got a few disturbed joints in the SMT reflow ovens, interesting effect.
Maybe we could use solderpots like the Richter scale. The farther solder is
thrown from the pot the greater the intensity of the quake. The square of
the distance from the pot equates to the magnitude or something like that.


Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-356-6076

-----Original Message-----
From: Jonathan Boyle [mailto:[log in to unmask]]
Sent: Wednesday, February 28, 2001 2:03 PM
To: [log in to unmask]
Subject: [TN] Wave solder and earthquakes.


Not a question for you, just a statement...
Try not to be around a wave solder machine when an earthquake hits! Our
solder bath (located in Seattle, Wa.) did it's impersonation of a Hawaiian
surfers dream. Fortunately the operators were at lunch. Solder spills were
found 6 feet away! Now it's clean up time...

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2