TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 18 Dec 2006 10:23:12 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (38 lines)
 
Hi all,

This time it seems as the article is not so old as the one I used some
weeks ago. 
Now, the Lead amount and recycling efficiency is little different, but
still disadvantageous compared to Tin, Copper, Gold and others. Still, I
can't understand how one can recycle 70% of the Tin from the soldered
boards, while only 5% of the Lead, in one and the same recycling
process.

http://www.sclf.ca/hazards.php

http://www.recycleworks.org/ewaste/ewaste_process.html


According to the below link, the (general) Lead recycling efficiency is
95% !! 

http://pubs.usgs.gov/of/2001/of01-170/of01-170.pdf


Do the green organisations present statistics? I still doubt....


Inge
SMW

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2