TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 20 May 2010 23:31:43 +0200
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=response
From:
Parts/Attachments:
text/plain (103 lines)
I forgot.  There is in fact a metal connection, sort of, that fuses without 
explosion, soot and splashing metal drops.  When too high current passes, it 
breaks, nicely and with no dramatic aftermats. You are all a foot or two 
from it every day, most of you half an hour in the morning and half an hour 
or so in the evening. What do i think of?
No, no, no.. Dave Hillman....not you again.  Let others guess first.  Yes, I 
know you are a MENSA member...
Inge

--------------------------------------------------
From: "Inge" <[log in to unmask]>
Sent: den 20 May 2010 20:37
To: "Glidden, Kevin" <[log in to unmask]>; <[log in to unmask]>
Subject: Re: [TN] Visual clues of over-current for leads

> Kevin.
>
> that was an odd question my friend. What benefit do you have of a 
> catastroph failure photo?  Sure, I have all kinds of photo material, but 
> to scan hundreds of reports to find a particular photo takes time. Instead 
> I go directly to your question.  It depends (Doug TM) on the kind of 
> circuitry you have. Resistive? Inductive? Current limitation? Lead 
> material? Heat paths?  Lead cross section area? Lead length? etc
>
> Let's compare with a gold bond 1 mil wire. Despite it's thinness, it's 
> capable of taking 6 amperes DC for some milliseconds. Then imagine a 
> component lead!!   Maybe a hundred amperes instantly.  Overcurrent can 
> appear as a) a inrush current high enough to rise the resistive current so 
> fast that you melt the lead within milliseconds.   The temperature reaches 
> thousands degrees and the hottest part of the lead vaporises.  Typically, 
> it acts like an explosion. Melt metal spreads around, oxides and soot 
> covers the surroundings and there is a smell of burnt material. The 
> voltage drops, some major fuse breaks and nothing more happens.  This  is 
> the most positive scenario.  What is far more dangerous is if the voltage 
> does not drop (it can increase instead, inductive load) but continues to 
> feed, arcing can start and put fire to surrounding components.  So, my 
> answer is: if the overcurrent disintegrates a lead, there will NOT be left 
> a smooth and clean metal, because that is against all physical laws.  With 
> one exception. Theoretically, if the short circuit current  is 'unlimited' 
> and dt/T is 'zero' , the lead may break by electromechanical forces rather 
> than by thermal causes.  The inventors have tried for may years to design 
> fuses that behave like that.  If your leg broke by overcurrent and is 
> still smooth and clean, hurry , take patent .
>
> My two amperes
>
> Inge
>
>
>
> --------------------------------------------------
> From: "Glidden, Kevin" <[log in to unmask]>
> Sent: den 20 May 2010 19:53
> To: <[log in to unmask]>
> Subject: [TN] Visual clues of over-current for leads
>
>> Hello,
>>
>> Can anyone describe or provide photos of what one might expect a lead 
>> that has been subjected to such a high current that it damaged (burned? 
>> disintegrated?) the lead?
>>
>> Would you expect to see charring all the time?  Is it possible to see 
>> smooth, clean surfaces with just a section of the lead missing?
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to 
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives
>> Please visit IPC web site 
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
>> ext.2815
>> ----------------------------------------------------- 
> 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2