Steve,
Thank you for sharing.
You did not comment on the moisture inquiry. I heard that moisture can penetrate to the conductive ink and cause corrosion. By the way how thick is this coating or min requirement.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Thursday, June 23, 2011 1:05 PM
To: [log in to unmask]
Subject: Re: [TN] Ceramic resistor coating
Victor,
Chip resistors normally have a low temp firing glass over the resistive
element, or sometimes an organic, epoxy based material. You would
ultimately have to check with your supplier to determine which. .... or dig
at it [destructively] under a microscope to estimate for yourself.
The glass resistor covercoat normally fires at 500-525°C, so it will not be
bothered by much of anything which you can do to it.
The organic covercoat would act like a standard epoxy and could discolor,
change color, crack, peel, etc with excess temps, or could have issues with
solvents, etc.
Hope this helps
Steve Creswick
http://www.linkedin.com/in/stevencreswick
616 834 1883
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, June 23, 2011 12:16 PM
To: [log in to unmask]
Subject: [TN] Ceramic resistor coating
Fellow TechNetters:
What are some typical ceramic resistor coating? Are these coating
moistures proof/resistance? Can the coating deteriorate with temperature?
Victor,
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|