TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 9 Sep 2002 12:22:38 -0700
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="Windows-1252"
MIME-Version:
1.0
Parts/Attachments:
text/plain (145 lines)
What are we looking in the ball photo? Are these voids caused by a test
socket? What testing was the device subjected causing these voids? And
lastly is the damage detected before attachment to the board?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of
[log in to unmask]
Sent: Monday, September 09, 2002 10:27 AM
To: [log in to unmask]
Subject: Re: [TN] 1mm bga voiding


Victor and other Technetters,

Hopefully this link shows the 1mm BGA picture (x-section)

http://www.ofoto.com/PhotoView.jsp?UV=922011120789_31499403105&US=0&collid=2
9888403105&photoid=19888403105


Al




Victor Hernandez <[log in to unmask]>@IPC.ORG> on 09/09/2002
12:23:59 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:

Subject:  Re: [TN] 1mm bga voiding


Al,

   The IPC-A-610C sec. 12.2.12 Area Array/Ball Grid Array states that "
Acceptable - Class 1,2,3 Less than 10% voiding in the ball to board
interface.   Process Indicator - Class 2,3  10-25% voiding in the ball to
board interface.   What is the SIZE of the ball you are using.

   Did we have to SIGN UP to the Web Page to view your photo.   Perhaps a
fellow TechNetter can offer their site for viewing.

victor,

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, September 09, 2002 9:13 AM
To: [log in to unmask]
Subject: [TN] 1mm bga voiding


Technetters-

We are getting 1mm BGA devices with these mechanical defects (see attached*
for link to picture) from testing processes at the vendor.

These devices have excessive voiding when reflowed on to a board with other
BGAs that do not have a voiding problem.  The vendor insists it is our
process that causes the voiding.

Question-  would you expect this mechanical damage to lead to voiding in
the reflowed joint?


*
http://www.ofoto.com/ShareLandingSignin.jsp?UV=922011120789_31499403105&US=0

&Upost_signin=OrderPhotos.jsp%3FshowSlide%3Dtrue&Un=774560513&Um=54718403105

.84079403105



Al

----------------------------------------------------------------------------

-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------

-----

----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2