TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Roger Massey-G14195 <[log in to unmask]>
Date:
Thu, 1 Apr 1999 10:15:12 +0100
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Roger Massey-G14195 <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
     Benny,

        As a bonder, I dont know much about electroplating but I do know
     that a lot of places tend to spec a sulfamate layer. I understand this
     is because the sulfamate is a more ductile layer, and hence less prone
     to cracking during service etc.  A couple of important notes, the
     plating should be free of organic brighteners and relatively pure Ni
     (99%min) and , as these can screw up the initial bondability and also
     the long term reliability respectively

        Without knowing the exact lay-up the platings, I dont know if you
     are bonding onto the Ni iteslf, or a thick layer of soft Au, if onto
     Au, the Ni underneath should'nt matter too much, as long as the Au is
     well adhered and the Ni doesnt crack.
        If going direct onto the Ni itself, I would go for a more ductile,
     and softer layer. difficult I know, but try and "match" the hardness
     of the Ni to that of the wire, as this will minimise the damage to the
     wire during bond, and go for a ductile layer which will withstand the
     U/S energy without cracking.

        Its difficult to give a green light to either system, I know people
     who bond onto both layer types succesfully, with similar machines and
     wires.

        Having said that, I would be interested in the response from any
     plating gurus out there as to the differences between the two layers,
     I kinda know what works out on the floor, It would be neat to know why

                        Regards.
                           Roger

______________________________ Reply Separator _________________________________
Subject: [TN] Ni Plating for wire bond
Author:  "TechNet E-Mail Forum." <[log in to unmask]> at #email
Date:    01/04/99 10:23


Hello Everyone,

What kind of chemistry do you recommend for electrolytic Ni plate, sulfamate
or sulfate nickel, as applied on thermosonic wire-bond PCB? I was told long
time ago that sulfamate nickel is a 'low-stress' nickel being used in
various metal finishing jobs, including PCB; while the latter comes from a
Watt nickel bath. Some BGA designers says that as long as the metal surface
is clean, the two nickel types should work equally well.

I recently tried both and found that the sulfate nickel has a better
bondability, despite the fact that they come from two different vendors.

Can anyone tell me about the surface topography of each type of nickel? Do
they have different atomic packing in the plated layer? What actually does
low/high -stress mean, something related to hardness? Assuming they have the
same amount of gold plated on top, which one is more suitable for gold wire
ball bond?

Thanks in advance!

Regards, Benny.

Wire Bonder Process Eng'g
ASM Assembly Automation

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2