Werner,
The data sheet lists the insulator material as LCP. The pins are stated
to be a copper Alloy with Gold over Nickel.
Leif Erik Laerum
Quality Assurance Manager
Texas Memory Systems
[log in to unmask]
Tel: (713) 266-3200 x468
www.texmemsys.com
Werner Engelmaier /* wrote:
> Hi Leif
> You do not say how long that connector is and what the connector body material is.
> My guess on very skimpy info is that you have a too long connector made with an unsuitable connector body material, with connector pins made of some connector pin metal, like BeCu, that while it is a good connector pin material with good spring characteristcs, it makes for bad solder joints
>
> Werner
>
>
>
>
>
>
>
> -----Original Message-----
> From: Leif Erik Laerum <[log in to unmask]>
> To: [log in to unmask]
> Sent: Fri, 15 May 2009 5:16 pm
> Subject: [TN] Connector with loose pins
>
>
>
>
>
>
>
>
>
> Technetters,?
> ?
>
> I have a less scientific question, but I hope someone has some
> experience with a similar problem.?
> ?
>
> We have a .090 think motherboard where one particular part number
> connector frequently have loose pins. It is 33 cm by 16mm. There are
> lots of other types of connectors on the board that does not have
> issues. We only have problem with one part number. These connectors are
> at the very front of the board. They go in the oven first. This is a
> leaded solder board and we use SN63/Pb37 solder. The loose pins tend to
> be at the end of the connector and on power planes. On some boards it
> appears that the connector sort of twists or bows a little bit.?
> ?
>
> The problem is that this surface mount connector is very hard to fix.
> The pins frequently short and due to space limitations, it is hard to
> reach them with the tip of the soldering iron. They also tend to develop
> shorts easy. This makes it even harder to fix after reflow.?
> ?
>
> We have tried reducing the cooling at the end. We have sent the boards
> through the oven with the mate installed in order to stiffen up the
> connector. The profile was checked as late as today. Nothing jumped out
> at me.?
> ?
>
> Does anyone have experience with a similar problem that they managed to
> solve??
> ?
>
> Thank you.?
> ?
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|