TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Haynes <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 12 Mar 1999 10:55:03 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
Short note:
Magnetic interactions stop about kHz because the magnetic perm.. coffficient
goes to 1.
Thanks for relating your data.
Richard Haynes

-----Original Message-----
From: Barry Bates <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, March 12, 1999 4:21 AM
Subject: Re: [TN] Effect of Surface Finish on RF Boards


>Michael,
>We have experienced unacceptable loss at 3GHz for 50 ohm
>microstrip transmission lines with the standard Ni Au finish on
>1/2 oz and 1oz copper using Rogers and Arlon PTFE based
>substrates.
>What we found OK was a cheat, we applied the standard Ni Au
>finish to all the exposed pads, ie solder, test, contact, etc.
>and we left the rest of the track bare Cu with the normal, thin
>Probama solder resist coating. The solder resist had to cover
>part of the Ni Au to ensure sufficient environmental protection.
>The solder also adds to the attenuation budget so be sparing with
>it. The higher the frequency the worse it gets.
>As far as I recall, Ni also does some of its attenuation via a
>lossy magnetic interaction with the EM wave.
>This gave the microwave guys the performance they were after.
>The detail I do not have but I recall that the losses went from
>many tenths of a dB to just about 1/4 dB for about 450mm long 50
>ohm track
>Regards,
>                Barry Bates
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2