TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Thu, 7 Apr 2005 16:30:23 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (135 lines)
We have several products that use this style LED.  We do have more issues with them skewing but try to watch the layout or add just a drop of adhesive behind the dome to help keep it centered.  Luckily, we have had only minor issues with them and quickly became successful.  The solder joint we obtain is very good but we have had no products being subjected to HASS testing that I am aware of.  

Kat

>>> [log in to unmask] 4/7/2005 4:23:42 PM >>>
Hi Jack!

That was my first thought when I started looking at the issue, but they
indeed
are right angled LED's. Stanley (the manufacturer of the LED's) calls them
right
angled LED's, and you can see the silkscreen on the fab that shows which
way
the lense is supposed to face.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


|---------+---------------------------->
|         |           "Jack C. Olson"  |
|         |           <OLSON_JACK_C@cat|
|         |           .com>            |
|         |                            |
|         |           04/07/2005 09:24 |
|         |           AM               |
|         |                            |
|---------+---------------------------->
  >--------------------------------------------------------------------------------------------------------------|
  |                                                                                                              |
  |       To:       [log in to unmask]                                                                  |
  |       cc:       [log in to unmask]                                                                              |
  |       Subject:  Re: Right Angle LEDs                                                                         |
  >--------------------------------------------------------------------------------------------------------------|








Steve,

I assume when you show the picture "SMT TOP" that THAT is the orientation
you are soldering them?

From the way the terminations look (wrapped around the ends, nothing on the
sides) it almost seems like the manufacturer intended them to be soldered
in the orientation that you have labelled "LED PAD LAYOUT".

Are you sure those are right angle? and should be laying down on their
side?

just a thought....

Jack



----- Message from Stephen Gregory <[log in to unmask]> on Wed, 6
Apr 2005 08:55:39 -0500 -----

                 Subject: <No subject given>


Morning Everyone!

I just ran an assembly here that has some strange little right angle LED's
that I've never seen before. They were brought to my attention because
many of them were coming out of reflow pretty badly skewed. I've got a
few images of the LED at;  http://www.stevezeva.homestead.com

Look at "LED Top, LED Bottom, LED Pad Layout, and Recommended
Layout".

For one thing, you'll see that these LED's have no real termination to
solder to, except on the face of the ends. Another thing I discovered after
I went and checked the dimensions of the pad layout in the gerbers, then
compared it with the manufacturers recommendation, the layout isn't even
close to what's recommended.

My question is, what would you do to try and protect what little solder
joint
that is going to form, from being damaged? Some sort of glue bonding?

These little guys will need to withstand HASS testing in the upper-level
assembly believe it or not. But I'm not holding out much hope for that.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX





__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2