TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 14 Jun 2005 11:00:53 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Arciolla <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Bob Arciolla <[log in to unmask]>
Parts/Attachments:
text/plain (85 lines)
Hi Steve,

Your right on when you suggest using loaf pans for emptying the pot. We use
a ladle and loaf pans and it really works great.

Bob Arciolla
Endicott Research Group
Quality/Safety Manager
----- Original Message -----
From: "Stephen Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, June 14, 2005 10:29 AM
Subject: [TN] Emptying Wave Solder Pots...


> Well, we're emptying our 1800-lb Electrovert Electra solder pot
> today.
>
> If you remember, I posted about a week ago of our maintenance
> breaking off one of the wave former hold-down bolts doing his weekly
> maintenance, and the only way to fix it is to empty the pot.
>
> I remember not too long ago, a post asking about how does one go
> about emptying a wave solder pot. So I though I'd take some pictures
> of our little task today, and how I go about doing it, then  post them on
> my web page. Go to: http://www.stevezeva.homestead.com and click
> on "Picture Page 2", then look at "Emptying Pot and Emptying Pot 2".
>
> Like I said a while back, I don't use a pot drain, I feel they're just too
> dangerous. As you can see in Emptying Pot 2, our pot does have a
> drain, but I won't use it.
>
> I just set-up a nice sturdy table, with a piece of metro rack shelf on top
> of it, then using "Bakers Secret" loaf pans (you have to use "Bakers
> Secret" loaf pans, the teflon coating is bullet proof!), carefully ladle
> the
> solder into the pans to create your solder ingots.
>
> You can see the first beauty in the first picture. I'll post a picture
when
> we're
> done.
>
> Kind regards,
>
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and confidential
to
> LaBarge, Inc.  It is for use only by the individual or entity named above.
> If you are not the intended recipient, you may not copy, use or deliver
> this message to anyone.  In such event, you should destroy the message and
> kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2