Hello Technet world,
I'm looking for non destructive method to measure copper thickness in small
holes such as .020 inch and smaller. If anyone ever saw some equipment that
has this capability, I would certainly appreciate some feed-back off-line.
Thank you all for your support,
Charles.
Charles Desroches
Technical Advisor
Viasystems Canada inc.
379 Brignon Street
Granby, Quebec, Canada
J2G 8N5
Voice: 450-372-8111 (2257)
Fax: 450-378-5110
[log in to unmask] <[log in to unmask]>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|