TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Inge Hernefjord <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Date:
Fri, 23 Mar 2012 18:12:31 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
I don't know NASA's routines. European satellites use to be run for  x  hs
before launching, It's  done in order to cut the familiar early failures in
the start of the   'bath tub ' curve. Maybe, whiskers do not grow so
fast in these tests as being in the orbit.

/Inge

On 23 March 2012 15:36, Bob Landman <[log in to unmask]> wrote:

> Steve,
>
> I asked Henning about a satellite that failed in orbit due to whiskers as
> to how they could possibly deduce that when I saw him at the CALCE meeting
> at UMd.  He told me it was because they had similar equipment on the ground
> and could verify that whiskers had likely erupted.
>
> Bob
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
> Sent: Thursday, March 22, 2012 4:50 AM
> To: [log in to unmask]
> Subject: Re: [TN] Out of the world tin whiskers
>
>  Bob,
>
> Yes, will be very interesting to hear what the group can share.
>
> Could it be possible they still have a back-up/alternate CAPS instrument/s
> in storage to physically examine for whiskers, thereby making the problem
> definition a bit easier.
>
>
> Steve C
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2