Doug,
It appears that they flooded the area for a component with the flux
prior to soldering the component. I have always recommended the use of
No-clean flux pens that are used only on the pads (or the row of pads
for fine pitch devices) the flux pen limits the amount of flux that is
applied to the board, as well as limiting the area where the flux
remains.
In this case the assembly house did not do this.
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, April 23, 2012 7:57 AM
To: TechNet E-Mail Forum; Woolley, Mark D. (Mark)
Subject: Re: [TN] No-Clean Flux
Mark,
In my opinion, no, it is not acceptable to leave these materials on a
circuit board. I have found them to be electrically conductve when
unactivated and can be corrosive.
How are you adding flux in the rework and touch up? If you are
squirting on large volumes, I think you have a problem. If you are
using a needle point dispenser that applies a drop at a time you are
probably OK. Another possible alternative is to use fillable flux pens
that have a fine paintbrush type tip.
Doug Pauls
From: "Woolley, Mark D. (Mark)" <[log in to unmask]>
To: <[log in to unmask]>
Date: 04/23/2012 08:43 AM
Subject: [TN] No-Clean Flux
Sent by: TechNet <[log in to unmask]>
________________________________
I have an issue with one of the assembly houses we use. They are using
a No-clean flux that contains adipit and succinic acids (per the MSDS)
in an alcohol base.
Is it allowed to leave flux on the PWB that HAS NOT BEEN DEACTIVATED BY
HIGH TEMPERATURES OF SOLDERING?
I am not talking about the flux used in the solder paste or wave
soldered flus. I am talking about the flux used at rework and touch-up
of the PWB.
I havce seen papers detailing corrosion on PWBs using "no-clean" fluxes
and I have seen it on some of our products. This usually pccurs near
the periphery of the PWB where the wave solder flux is protected by the
pallet used to pass the PWB through the solder wave.
Any opinions and references will be appreciated. I can give the
manufacturer and flux type to individuals, but don't want to put it in a
global email.
Thanks
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|