TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Reid <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Date:
Tue, 4 Nov 2008 14:26:13 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Hi Charming,

Two points:

1. The extra thermal excursion at lead free reflow temperatures is a
reliability concern. It is one more thermal cycle that is degrading the
dielectric and the copper. I have seen one extra lead free thermal cycle
have a significant influence on reliability. The quality of fabrication
including copper quality (thickness, distribution etc.), dielectric
robustness and design influences, like grid size, all conspire to
establish the reliability in lead free applications.  

2. A nickel finish usually extends reliability by protecting the PTH
from producing significant barrel crack. So expect the reliability of
the PTH to be reduced by not having nickel protection.

The most conservative approach is to do thermal cycle testing to confirm
or refute reliability of you product in your application.

Sincerely,

Paul Reid

Program Coordinator

PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario
Canada, K2H 9C1

613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask] <mailto:[log in to unmask]>


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charming Chan
Sent: Monday, November 03, 2008 10:45 PM
To: [log in to unmask]
Subject: [TN] Build backplane with lead free HASL surface finish?

Hello TechNet experts, 

On our master fabrication drawing, the surface finish for backplane is
specified as ENIG, but the fabrication shop ask for waiver to build with
lead free HASL. Is it reliable enough? Any other concerns should be
taken into consideration? Thanks a lot.

Best Regards
Charming Chan
PCBA Engineer

--------------------------------------------------------
ZTE Information Security Notice: The information contained in this mail
is solely property of the sender's organization. This mail communication
is confidential. Recipients named above are obligated to maintain
secrecy and are not permitted to disclose the contents of this
communication to others.
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this email in error please notify the
originator of the message. Any views expressed in this message are those
of the individual sender.
This message has been scanned for viruses and Spam by ZTE Anti-Spam
system.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2