TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 26 May 1999 09:06:39 -0700
MIME-version:
1.0
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Yu-Shan Han" <[log in to unmask]>
Content-type:
text/plain; charset="iso-8859-1"
Subject:
From:
Yu-Shan Han <[log in to unmask]>
In-Reply-To:
<91B504DF04CCD211821D0008C733EADF04F4FD@HSFEX135>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (60 lines)
Hi Jonathan:

This is from MSDS of Phibro Tech's High Speed Ac-cu-Guard:

NH4Cl       19 - 27 %
NH4OH       14 - 23 %
NH5CO3       1 -  5 %

Sp. gr.:        1.015 - 1.045
Vapor pressure  96 mmHg
pH      9.4 - 10.4

Hope this'll help.

Yu-Shan Han

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Meigs, Jonathan
Sent: Wednesday, May 26, 1999 6:47 AM
To: [log in to unmask]
Subject: [TN] Ammoniacal Etchant Recipe


Good Morning, Everyone!

I am in need of a quick and dirty recipe for an ammoniacal etchant for use
in one of my lab experiments. I'm not trying to make 2 mil lines and spaces,
but it needs to be ammoniacal.

Can anyone help me with a recipe?

Thanks in advance,


Jonathan Meigs
Product Development Engineer

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2