TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 12 Nov 2010 15:12:39 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
Subject:
From:
Bob Landman <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0 (iPhone Mail 8B117)
Parts/Attachments:
text/plain (162 lines)
Ha!! Love that show.

Bob

Steve writes:

> Direct communications, should anyone with to negotiate the details of their coating's doom, can go to [log in to unmask] .
> 
> Best
> 
> Steve

Sent from my iPhone

On Nov 12, 2010, at 2:32 PM, [log in to unmask] wrote:

> It really has to be tough working in a technical industry with the name
> Steve Smith, as a Red Green fan the first thing I thought of was duct
> tape...  
> 
> Keep your stick on the ice,
> - Graham
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
> Sent: Friday, November 12, 2010 2:54 PM
> To: [log in to unmask]
> Subject: Re: [TN] UV radiation and conformal coating
> 
> Doug,
> 
> I sent your posting to an old college friend who is a physicist with a
> great deal if working knowledge on chemical finishes as his company
> makes paints and protective coatings for the marine environment.  He is
> teamed with Bill Rollins at Raytheon Tucson on a grant from the MDA to
> develop a whisker-tough conformal coating. 
> 
> He replied:
> 
> Bob,
> 
> Thanks for forwarding this to me.  I am not subscribed to the list, so
> please post this for me.
> 
> All,
> 
> Varnish fails on wood of boats in one or a few years, due to the
> ultraviolet of the sunlight eventually getting thru the varnish [even
> with UV absorbers] and breaking down the cellulose of the wood below.
> Cellulose has a lot of carbon-carbon and carbon-oxygen bonds.
> 
> Indeed; the loss of gloss of varnish is due to surface-oxidation by the
> solar ultraviolet photons breaking the atomic bonds of the
> material at the surface; those surface free radicals react almost
> immediately with atmospheric oxygen, and are literally burned away.
> 
> A carbon-carbon bond has an energy of about 348 kilojoules per mole, and
> will readily break with a barely-ultraviolet photon.
> 
> A carbon-oxygen bond has an energy of about 360 kilojoules per mole, and
> a carbon-hydrogen bond about 413.  For more details, see
> http://www.science.uwaterloo.ca/~cchieh/cact/c120/bondel.html .
> 
> Ultraviolet and even blue-visible photons have enough energy to break
> these bonds.
> 
> Broken atomic bonds create free radicals, and some of these will bond
> onto neighboring polymer chains, causing increased modulus, reduced
> elongation, and in fact the polymer gets smaller. the reason flakes of
> paint curl outwards when they fail is that the outer surface has more
> tensile stress than the material below, due to free-radical damage at
> the sunlight-exposed surface. So, you see, it's going on all the time
> the sun shines.
> 
> Your conformal coating (made of carbon, hydrogen, oxygen and nitrogen
> and perhaps other atoms) is doomed; it's only a matter of time.
> 
> Steve Smith
> Www.smithandcompany.com
> 
> 
> 
> On Nov 11, 2010, at 8:20 AM, Douglas Pauls <[log in to unmask]>
> wrote:
> 
>> Good morning all,
>> 
>> Does anyone know of any papers on the effects of UV light on conformal
> 
>> coating?  Not talking the cosmic radiation hard space kind.  I know it
> 
>> would be wavelength and intensity specific.  Got a question from one
> of 
>> our engineers and I, of course, gave the very intelligent answer of
> "Beats 
>> me".  But I have this wonderful resourse called Technet...............
>> 
>> Doug Pauls
>> 
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
> [log in to unmask] 
>> ______________________________________________________________________
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
>> -----------------------------------------------------
>> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
> 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2