TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Fri, 12 Jan 2007 11:24:44 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (56 lines)
That looks just like an Ohio State Buckeye.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, January 12, 2007 9:30 AM
To: [log in to unmask]
Subject: [TN] Test Technician's Friday Surprise!

Yay it's Friday!!!
 
Well, I did all my grocery shopping yesterday so I could hole-up in my
apartment this weekend to sit out the ice storm we're gonna get here.
The temperature this morning was 65 F. when I got up this morning for
work 5-hours ago, now it's 30 F.. It's supposed to eventually get down
in the teens and we're supposed to get freezing rain starting in a few
hours and lasting until Sunday. I hope we don't lose power...
 
Anyways, one of our test technicians came to me just a little while ago
and told me he got the bejeebers scared out of him this morning. This is
why:
 
http://stevezeva.homestead.com/files/Holy_Sh_t.jpg
 
It would have scared me too. Don't know why this happed yet...and yes,
the part was installed correctly.
 
-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2