Similar experience - 1970 - Pigment production recipe called for one quart of Triton X-100 per pigment batch to keep finely ground pigment particles from re-agglomerating. We think the operator took 5 gallons from a drum, poured the quart into the mix, and dumped the other 4 3/4 gallons down the drain. Overfoamed our waste treatment plant, and then the very stable foam lifted sewer manhole covers a mile from the plant. Nice to have red foam, green foam, and blue foam at various points going away from our plant.
Think that Triton X-100 had uses in IR fusing fluid and maybe soldering flux in the dinosaur age of circuit board production.
Denny Fritz
-----Original Message-----
From: Brian Ellis <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Tue, Jan 18, 2011 7:23 am
Subject: Re: [TN] Avionics Fire Fighting Foam
Water-soluble soldering oils at 5% solution can act similarly! I
emember a PCB manufacturer client who had just switched to one, umpteen
ears ago, for tin-lead plating reflow, and they had a complaint from
he local sewage works, about 1 km away. Foam was coming out of an
gg-section sewer in an almost rigid extrusion! They sent two men with
reathing apparatus up the sewer to find out where the hell it was
oming from!
Brian
On 18/01/2011 00:17, David D. Hillman wrote:
Hi folks! I know this is going to sound weird but I am looking for some
assistance in finding out the product name(s) for the fire fighting foam
that is used in aircraft hangers. The foam appears like soap suds and can
fill an aircraft hanger very fast. Please send me the product name or a
possible contact I could call to talk to about fire fighting foam.
Thanks in advance
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|