TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 5 Feb 2008 10:53:14 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"Victor G. Hernandez" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (105 lines)
It would be great if vendor 1 & 2 photos of the same site were side by
side.
To me both x-sec exhibit microvoiding.

Victor


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, February 04, 2008 3:54 PM
To: [log in to unmask]
Subject: Re: [TN] Microvoids immersion silver

Hi Gaby!
 
Just got it up on my site now. I've been buried with my head in our VCD
all day pulling all the tooling out out to do an annual PM. But go to:
 
http://stevezeva.homestead.com/files/ImAG_from_2_vendors.doc
 
Steve

________________________________

From: Gabriela Bogdan [mailto:[log in to unmask]] 
Sent: Monday, February 04, 2008 1:55 PM
To: [log in to unmask]; [log in to unmask]; [log in to unmask];
Gabriela Bogdan; Lee parker
Cc: Steve Gregory; stephen gregory
Subject: Re: [TN] Microvoids immersion silver


Finished my "investigation". Attached word doc,  Steve, could you put it
on your site?
Can anybody comment or give an advice?
Thanks,
Gaby

	----- Original Message ----- 
	From: Gabriela Bogdan <mailto:[log in to unmask]>  
	To: [log in to unmask] ; [log in to unmask] 
	Sent: Tuesday, January 29, 2008 8:49 PM
	Subject: Re: [TN] Microvoids immersion silver

	Decided to investigate further to qualify our vendors.
	4BGA + 2 circuits and assembly.
	Will cross section bare, after paste+reflow, after BGA assembly
and also X-ray and dye and pry.
	At least I will have fun.
	Gaby

		----- Original Message ----- 
		From: [log in to unmask] 
		To: [log in to unmask] ; [log in to unmask] 
		Sent: Tuesday, January 29, 2008 8:35 PM
		Subject: Re: [TN] Microvoids immersion silver

		Hi Gaby,
		I take it what you are seeing are 'champagne voids.'
		Voids like these are 'encouraged by rough topography
copper, excessive Ag thickness, some solder paste choices and rapid
cool-down after reflow. But as Donald Cullen says in his comprehensive
paper, it "requires the "Perfect Storm" of a rather contrived
combination of parameters" to produce planar micro-voiding.
		Well Gaby, now you know it-you are "Perfect." ;-)
		
		
		
		Werner
		
		
		
		**************
		Start the year off right. Easy ways to stay in shape.
	
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2