Hi Neil! I recommend you take a look in JSTD-002B, section 4.3 for
information on wetting balance testing. Currently the wetting balance
testing procedure is a test without established accept/reject criteria. The
wetting balance test methodology in JSTD-002B does include some suggested
criteria which can be used. A number of companies are currently using the
wetting balance methodology as their solderability test method as they have
created agreed criteria values between themselves and their component
fabricators. The JSTD-002 committee is currently looking at creating
industry acceptable wetting balance accept;/reject criteria limits but it
is too early in the studies to know if we can achieve valid limits for
industry wide application.
Dave Hillman
JSTD-002 CoChair
[log in to unmask]
Neil Flatter
<Neil.Flatter@TRW To: [log in to unmask]
.COM> cc:
Sent by: TechNet Subject: [TN] Wetting Balance Testing
<[log in to unmask]>
05/08/2003 12:17
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Neil
Flatter
For those of you doing solderability testing, what sorts of parameters
should we be concerned about for reliable results? Our tester already
allows inputs for lead perimeter, cross sectional area, and hang time. My
company's testing also specifies immersion angle, depth, and speed as well
as the type of flux. By controlling these factors, can I expect repeatable
results?
It has been suggested that we also need to limit the length of the leads
for our testing as wall as installing a thermal break between the lead and
the hanger. Both have been blamed for failing test results. Has anyone
experienced changes in test results from these variables?
Neil Flatter
TRW-Automotive
Process Quality
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|