Ken,
A couple of notes about cutting phosphor bronze connector pins.
1. phosphor bronze does not take solder well, if at all.
2. By definition, you do not cut pins, only leads. As such, they do not have to be cut to meet maximum lead length.
I can honestly say I have not visited this issue in a number of years and do NOT have a copy of J-STD-001 or 610 at hand. Will one of you certified instructors please correct me if things have changed since WS6536C.
Steve Mikell
[log in to unmask]
----- Original Message -----
From: "Bloomquist, Ken" <[log in to unmask]>
To: [log in to unmask]
Subject: [TN] Connector Lead Trimming
Date: Wed, 13 Jul 2005 07:16:03 -0700
>
> Good Morning Technetters,
>
> We have some 15 and 25 pin D-sub connectors that we need to trim the
> leads. They are .030" phosphor bronze and we only need to trim about
> .020 - .030 from the ends.
>
> Does anybody know of some good reliable, low maintenance trimming tools
> that would work good for this application? I want to trim them pre wave
> solder, not post solder with a bologna slicer.
>
> Thanks,
>
> KennyB
--
___________________________________________________________
Sign-up for Ads Free at Mail.com
http://promo.mail.com/adsfreejump.htm
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|