TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Charles Barker <[log in to unmask]>
Date:
Fri, 11 Sep 1998 15:55:33 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Ken Patel <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (73 lines)
Ken,

I'm not sure where it would fit in, but you might want to reference
IPC-4101, "Specification for Base Materials for rigid and Multilayer
Printed Boards."

As you delve into 4101, you will find that you CAN get more specific in
specifying materials, if you feel you NEED to.

Good luck.





Ken Patel <[log in to unmask]> on 09/11/98 01:45:16 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Ken Patel <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Charles Barker/US/I-O INC)
Subject:  [TN] Fab note for Laminate material




Currently my fab note says...
MATERIAL: X THICK GLASS EPOXY, NATURAL COLOR, LAMINATED NEMA GRADE FR-4, 1
OUNCE COPPER.

I believe above is for regular material with Tg of 110C but I want to use
high Tg material, so how should I rewrite it...like

MATERIAL: X THICK GLASS EPOXY, NATURAL COLOR, LAMINATED NEMA GRADE FR-406,
TETRA II OR EQUIVALENT SUBSTARTE MATERIAL WITH MIMIMUM 165 DEGREE C Tg, 1
OUNCE COPPER.

or something different.

re,
Ken patel
______________________________________________________
Ken Patel                       Phone:  (408) 490-6804
1708 McCarthy Blvd.             Fax:    (408) 490-6859
Milpitas, CA 95035              Beeper: (888) 769-1808

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2