Once you have done your dye penetrant what means/technique will you use
to determine how far and what direction the suspected crack propagated.?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Tontis
Sent: Monday, August 25, 2008 9:25 AM
To: [log in to unmask]
Subject: [TN] Cracked component leads
I would like to do a dye and pry on some component leads that have
cracks in
them and see if I can measure how far the dye penetrates the crack. If
someone could point me in the right direction of a company that could do
something like this I would appreciate it.
Thank you,
Ted Tontis CID
Quality Engineer
Borg Indak, Inc.
701 Enterprise Dr
Delavan, WI 53115
C 262-949-8887
P 262-245-3060
F 262-728-3788
[log in to unmask]
www.borgindak.com <http://www.borgindak.com/>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|