Hi Martin,
Actually, we've done it as a two step process laminate one side of flex.
cut it off from the backing FR-4, flip it over and laminate the other side.
When we developed it looked great. They were firing up the etcher and I
still need to those results.
I'll see if I can come up with a source for Duofoil.
Thanks for the feedback.
Hans
-----Original Message-----
From: Martin Christie [mailto:[log in to unmask]]
Sent: Wednesday, September 27, 2000 11:52 AM
To: [log in to unmask]
Subject: Re: [TN] Flex Wrinkling during Hot Roll Photo Resist Laminatio
Hans,
Do you still get good adhesion of the resist using the FR4? My only concern
would be that the FR4 would tend to insulate the flex from the bottom heated
roller. It may look okay but may manifest itself as poor line definition
when you come to develop / etch.
I've used a material called "Duofoil" in the past as a rigidiser for very
thin flex (can't remember who makes it). Basically it's just a thin Al sheet
(normally used in stack make-ups for laminating flex circuits).
Martin
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
27/09/00 16:18
>Martin and Bareboard,
>
>Thanks for the replies.
>
>We taped the flex to some 31 mil FR-4, ran it through the laminator and it
>worked!
>
>Now, I'll order some pressure sensitive film for the next time.
>
>Hans
>
>
>-----Original Message-----
>From: [log in to unmask] [mailto:[log in to unmask]]
>Sent: Tuesday, September 26, 2000 2:33 PM
>To: [log in to unmask]; [log in to unmask]
>Subject: Re: [TN] Flex Wrinkling during Hot Roll Photo Resist Lamination
>
>
>A pressure variation from one end of the roller to the other would be my
>guess.
>Just had the same problem. Found one of the idler gears in the machine had
>spit out a key and was slightly out of alignment, which was causing the
>roller to apply uneven pressure across the panel.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|