Jason,
Our soldering equipment manufacturer is one who is wanting to charge $200 to
receive a disk with a fix-it file on it that is then installed onto the
computer and will automatically run the first time the equipment is
activated after Dec 31, 1999 11:59PM.
You don't want to know my response! It was language that is not appropriate
for the Internet!!!
I am going to be expecting (and I better see and receive) to see a supply of
these so call $200 disks available for pickup at NEPCON later this month!!
They are the only one of our equipment manufacturers that has this nerve.
Good luck.
Richard Hamilton
Clemar Mfg. / Rain Bird
[log in to unmask]
> -----Original Message-----
> From: <Jason M. Smith> [SMTP:[log in to unmask]]
> Sent: Wednesday, February 10, 1999 10:19 AM
> To: [log in to unmask]
> Subject: Re: [TN] Y2k
>
> What is the industry seeing from their equipment manufacturers in
> reference to
> Y2K fixes on pretty recent machinery (less than 3 yrs old) i am curious
> as to
> see how many people are getting stiffed from fixes proposed by the
> equipment
> manufacturers and if some are charging much more than other and if some
> are even
> charging others at all......I think you all get my drift. I'd appreciate
> a
> response.
>
> Jason Smith
> Process Materials Engineer
> Lexmark Electronics
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|