Hi Paul,
Are these bare boards or have they been assembled?
Has anybody checked them out on an x-ray machine?
Hans
Air Force Material Command - We keep them flying!
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
> -----Original Message-----
> From: Chalmer, Paul [SMTP:[log in to unmask]]
> Sent: Friday, June 11, 1999 03:53
> To: [log in to unmask]
> Subject: Re: [TN] from jpl
>
> Here is some additional information on the suspected manufacturing problem
> from NASA:
> ***
> we have some circuit boards that have developed open connections when we
> apply pressure, heat or vibration.
>
> we destroyed one of the boards to create these cross sections.
>
> 40% of the via connections on one layer developed problems as depicted in
> the cross section photos.the cross sections illustrate the anomalies.
>
> the boards were designed to mil-275 (ipc 2221).
> material fr4 .093
> smallest trace is .008 air gaps .005
> 12 layers
> vias are .025 pad / .010 hole / annular ring .0075
>
> four of six parts look to have failed.
>
> ron
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|