TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 17 Sep 2003 06:49:23 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Charles Caswell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Charles Caswell <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
We had one of these to checkout last Fall. We found that the temp. recovery was slow compared to our Metcal. For most jobs the iron worked fine but when we tried to solder anything heavy we had problems. 

-----Original Message-----
From: Diamond, Pat [mailto:[log in to unmask]]
Sent: Wednesday, September 17, 2003 2:32 AM
To: [log in to unmask]
Subject: [TN] Pace soldering irons


Hi all,

We have just purchased some  of the new Pace Tempwise soldering irons which
are microprocessor controlled, we are having a few teething problems with
stability when checking the tip temperature.  Has anyone out there had any
experience with this problem?

We are using a Hakko 191 thermometer to check the tip temperature.

Thanks,

Pat

****************************************************************************
***************
The information transmitted is intended only for the person or entity to
which it is addressed and may contain confidential and/or privileged
material.

Any review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited. If you received this in error, please
contact the sender and delete the material from any computer.
****************************************************************************
***************
Pat Diamond
Senior manufacturing Engineer
Weston Aerospace                Tel:     +44 (0)1252  868194
124 Victoria Road               Fax:    +44 (0)1252 370298
Farnborough, Hampshire, GU14 7PW        Web    www.westonaero.com>
England         Email  mailto:[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2