Nowland,
Can they use an 'odd form' placement machine, like a Quad to grip the
outside of the POLA and achieve better placement?
Do they get any solder standoff after reflow? Since the device is
apparently too heavy to self-center, it seems like the 'balls' would be very
flat and the resultant joints not of great longevity.
See what the experts in the field suggest
Steve Creswick
http://www.linkedin.com/in/stevencreswick
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nowland, Russell Howard
(Russell)
Sent: Monday, March 22, 2010 3:57 PM
To: [log in to unmask]
Subject: [TN] TI/Emerson SMT Board Mounted Power
Hello Technetters,
I have a problem I hope someone out there has a solution for.
I have on a PCA that uses a Texas Instrument/(Emerson Power/Artesyn) (dual
sourced but part of the POLA) SMT board mounted power converter. The MPN is
PTH03050WAS. It is actually combination PTH and SMT. The device has 40 mil
diameter pins for PTH and to make it SMT they simply add a donut (solder
dam) on the pin and round the edges and call it a solder ball. I think the
problem my EMS is having is really with pick-n-place because the pick-up
point (Actually the top of a transformer) is off-center, fairly small, and
it has a plastic label on it.
The problem is the device is coming out of the oven skewed and violating IPC
610D. The pad diameter is exactly what is recommended by the datasheet
(.085-inches). The TI datasheet recommended a 0.080-0.085 diameter aperture
@ six mils. Originally my EMS had 0.085-inch @ 5 mils but changed the
aperture to a bull's-eye shape with the thought the bull's-eye would help
center the device. Both of the stencils have failed to draw the device to
the center.
Because this is really a Butt Joint I am holding the EMS to no side
overhang. This is causing them quite a headache. They have also not come up
with a viable solution either.
Here is the link to the data sheet
http://www.emerson.com/sites/network_power/en-US/Products/Product_Detail/Pro
duct1/Documents/PTH03050%20DC-DC%20Converter/PTH03050%20Data%20Sheet.pdf
Has anybody used these devices with good results? If so can you share your
methodology?
Thanks in advanced,
Russell Nowland
Alcatel-Lucent
Advanced Manufacturing Engineer
Address: 14000 Quail Spring Parkway, Suite 300
Oklahoma City, OK 73134
email:
[log in to unmask]<mailto:[log in to unmask]
>
Desk: 405-302-1660
Cell: 405-203-0034
Fax: 405-302-1622
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|