TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Date:
Fri, 18 Jun 2010 07:47:23 -0700
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Parts/Attachments:
text/plain (50 lines)
There are lots of different finishes for magnetic wire. You may have gotten
a high temp finish instead of what you are use to. Abrasion or high temp
solder are the best ways to remove it.

KennyB 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon (SA-1)
Sent: Friday, June 18, 2010 7:50 AM
To: [log in to unmask]
Subject: [TN] REMOVING VARNISH ON TRANSFORMER

Have a issue with a very small transformer that the varnish is near to
impossible to remove from the end of the wire.  In the past we did not
have a problem and yes we are going to contract the manufacture but they
are closed on Fridays. 

 

The specification for the wire to be used is RM5P-CB1-6 and I have been
unable to find it searching the internet.  Some transformer the varnish
did come off with heat from a soldering iron but several were not
affected by heat.  Scrapping is not what I prefer and even when the
operator tried that it was difficult to almost impossible to remove.  

 

Question:  could it be the incorrect wire used or a defect in the
varnish applied or that process to apply the varnish?  Just picking your
brains on a Friday, Thanks for any suggestion and I will let you know
next week what we find out from the manufacture of the transformer.  Jon




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2