Hi Technos,
for a couple of days I see occurences of blowholes in the joints of, guess what, SMT 0603 resistors.
The reflow recipe did not change and we're talking about 2 different established products, we have run many of each before. One is WS, the other one no-clean. Each one uses different brand of solder paste, SnPb.
I have changed the paste with fresh one, no positive results. I have changed the reels with different date codes, Bingo! But even the "bad" parts were quite fresh, less than one year old. One of them is pure Sn plated, don't know about the other ones.
The question is: where on Earth can humidity stay in a ceramic resistor? What else can be the cause of the blowholes? Did not bake the boards, since changing the components worked, so I guess the PCBs are out of the hook...
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|