Graham,
Those suppliers of our who make Al backed teflon boards do not strip the
zincate prior to E/L Ni. A strong caustic cleaner should activate the
aluminum surface. Back in a stone aged past life, we stripped anodized
aluminum using strong caustic.
Regards,
Dave Sullivan
Rockwell Collins
[log in to unmask] on 04/21/98 08:31:59 PM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Sullivan/CedarRapids/Collins/Rockwell)
Subject: [TN] Copper/Aluminium Clad Teflon Plating
Copper/Aluminium clad Teflon Plating
Specifically, my query concerns plating 0.5oz to 1oz copper on Teflon
with 1/8 to 1/4 Aluminium back (6061).
What is the best method of activating the Aluminium surface prior to
plating without using a nitric desmut, as this attacks the copper
surface.
or
What can be used for removing the smut on the Aluminium surface after
etching in a potassium fluoride etch which will not attack the copper
surface.
How can I achieve maximum adhesion of electroless nickel on Aluminium,
such as double dipping in Zincate. without stripping the Zincate with
Nitric
Thanks in advance
Graham Savage
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|