Subject: | |
From: | |
Reply To: | |
Date: | Tue, 15 Oct 2013 16:32:38 -0300 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Dewey
The quantity of layers and the pcb thickness don't increase the time of
baking?
In this IPC there is a simply table with Final Finish, but don't have
information about 'Thickness x #Layers'.
Thank you
_____________________________
Juliano Bettim Ribeiro
DATACOM
ENGENHARIA DE PROCESSOS
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000
+55 (51) 8446-2135
+55 (51) 3933-3000
Ramal: 3877
[log in to unmask]
www.datacom.ind.br
-----Mensagem original-----
De: Whittaker, Dewey (EHCOE) [mailto:[log in to unmask]]
Enviada em: Tuesday, October 15, 2013 4:17 PM
Para: TechNet E-Mail Forum; DATACOM - Juliano Ribeiro
Assunto: RE: [TN] IPC PCB Baking =[PCB Thickness x #Layers = 'X' hours @'Y'
°C]
Start with IPC-1601.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of DATACOM - Juliano
Ribeiro
Sent: Tuesday, October 15, 2013 12:13 PM
To: [log in to unmask]
Subject: [TN] IPC PCB Baking =[PCB Thickness x #Layers = 'X' hours @'Y' °C]
Hi to all,
I'm looking for which IPC that indicate the time to bake the PCBs with
problem in the HIC - Humidity Index Card.
We have PCB with single up to 16 layers, what time of baking if necessary in
these PCBs?
Is there a table with =[PCB Thickness x #Layers = 'X' hours @'Y' °C] in the
IPC ?
Could I use the table of IPC-033b?
Thank you a lot
_____________________________
Juliano Bettim Ribeiro
DATACOM
ENGENHARIA DE PROCESSOS
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000
+55 (51) 8446-2135
+55 (51) 3933-3000
Ramal: 3877
<mailto:[log in to unmask]> [log in to unmask]
<http://www.datacom.ind.br/> www.datacom.ind.br
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|