Years ago, when I was young... er, when we did hand taping, we used mineral
spirits, so any solvent containing mineral spirits would work. Use
sparingly with plenty of ventilation. (Somebody else will probably come up
with something better and chide me for adding to the environmental
pollution problem, oh well...)
Hope you find what yer' lookin' fer.
Roger M. Stoops, C.I.D., PCB Designer
Spectra Precision Inc.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511
Hinners Hans Civ
WRALC/LYPME To: [log in to unmask]
<Hans.Hinners@ROBI cc:
NS.AF.MIL> Subject: [TN] Adhesive Remover for artwork
Sent by: TechNet
<[log in to unmask]>
07/13/00 08:41 PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Hinners
Hans Civ
WRALC/LYPME
Hey Gang,
I'm looking for an adhesive remover.
We're using a new label printer to image the batch numbers on the panels.
Only problem, the labels are leaving adhesive on the artwork when we pull
them off. I already tried Chemtronics adhesive remover and it just smeared
the glue around. So, before I start making a bunch of calls or trying
household cleaners I thought I'd ask this illustrious body.
Thanks,
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials (Process & Manufacturing) Engineer
Warner Robins Air Logistics Center
Avionics Production Division
Manufacturing Branch
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|