Mark,
Most companies I've seen (numerous) use Mil-Std-883 Method 2017, Class H
(equivalent to the old Class B military - not Space, Class S, which is now
Class K). Even commercial operations generally use it as a guide. Current
revision is now at "E".
Regards,
Bruce Misner
> ----------
> From: Mark Gilbert[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Mark Gilbert
> Sent: Thursday, November 09, 2000 4:30 PM
> To: [log in to unmask]
> Subject: [TN] Die Attach
>
> This might sound like an elementary question to many of you but can you
> tell
> me what your companies use for a reference for standards in regards to die
> attach. Do you have your own standard or do you reference something from
> an
> organization such as IPC or the like? If it is in-house, are you allowed
> to
> disclose this information? This is unchartered territory for my company
> as
> we are expanding or product line (we previously have done very limited
> manufacturing here) and we are in the process of educating ourselves on
> this
> topic. Any input would be most appreciated.
>
> - Mark
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|