TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
X400-Content-Type:
P2-1988 ( 22 )
Old-Return-Path:
Date:
20 Sep 1996 17:48:32 -0500
X-Status:
Precedence:
list
Resent-From:
Conversion:
Allowed
Disclose-Recipients:
Prohibited
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Sat Sep 21 11:
48:15 1996
Status:
O
Priority:
normal
X-Loop:
X-Mailing-List:
<[log in to unmask]> archive/latest/6377
Content-Return:
Allowed
X400-MTS-Identifier:
[/c=US/admd=MCI/prmd=Honeywell/; 0168932431F40104-HW-MTA-AZ]
TO:
"[log in to unmask]" <[log in to unmask]> (Return requested)
Message-Id:
<0168932431F40104*/c=US/admd=MCI/prmd=Honeywell/o=AZ-MTA/ou=MSMail/ou=CAS/s=Edwards/g=Ted/i=A/@MHS>
Return-Path:
<TechNet-request>
MIME-Version:
1.0
X400-Recipients:
non-disclosure;
X400-Originator:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0v4EGZ-0000TIC; Fri, 20 Sep 96 17:41 CDT
Resent-Message-ID:
<"ZkIu41.0.zy5.gsnGo"@ipc>
Subject:
From:
"Edwards, Ted A (AZ75)" <[log in to unmask]>
Alternate-Recipient:
Allowed
X400-Received:
by /c=US/admd=MCI/prmd=Honeywell/; converted ( IA5-Text); Relayed; 20 Sep 1996 17:48:32 -0500 by mta HW-MTA-AZ in /c=US/admd=MCI/prmd=Honeywell/; converted ( IA5-Text); Relayed; 20 Sep 1996 17:48:32 -0500
Original-Encoded-Information-Types:
IA5-Text
Content-Identifier:
0168932431F40104
Parts/Attachments:
text/plain (61 lines)
Several of the chemistry suppliers are offering/implementing Palladium as an 
alternative to HASL or OSP.  They should be able to tell you who is in 
production.  Here are a couple of places to start

LeaRonal
David Marks
272 Buffalo Ave
Freeport, NY
516-868-8800

MacDermid
Michael Norwood
245 Freight St.
Waterbury, CT
203-575-7948

Another good contact is :
The former Bell Labs
Lucent Technologies
Bruce Stacy
908-582-4289
Or west coast
David Williams
408-249-8993

Hope this helps; [log in to unmask]

 ----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Ag or Pd alternative to HASL inquiry
Date: Friday, September 20, 1996 11:59AM


     What companies sell silver or palladium solderability coatings as an 
     alternative to HASL?
        What production PCB fabricators use either of these solderability 
     finishes?
        Thanks for any information regarding this matter.
              David Kelly
     Materials & Processes
     Boeing Defense & Space Group
     [log in to unmask]
     (206)773-7342

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2