TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 29 Jul 2009 09:54:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Victor Hernandez <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Unable to open provided URL address.   Perhaps a block at my employer.



Victor,



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*

Sent: Wednesday, July 29, 2009 9:50 AM

To: [log in to unmask]

Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT





 There is something called a Gold-Embrittlement 'Calculator' at M. Lau & T. Clifford, “Lockheed Martin Gold Calculator.xls,” see: http://circuitassembly.com/cms/content/view/3630/95/



Werner





 





 



-----Original Message-----

From: Steven Creswick <[log in to unmask]>

To: [log in to unmask]

Sent: Wed, Jul 29, 2009 10:31 am

Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT





















Guy,



You might try to contact Steve Z and see if he has the time to drop it into

his site.  I'm sure that it can't be all that large of a spreadsheet.  



Possibly it is already buried there somewhere.  I just took a quick peek and

did not see something in that line of thought.



Steve C





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey

Sent: Wednesday, July 29, 2009 10:23 AM

To: [log in to unmask]

Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT



Technet does not allow attachments but I have a spreadsheet that I picked up

from someone on Technet. It is dated 6/21/06.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon (SA-1)

Sent: Tuesday, July 28, 2009 8:54 AM

To: [log in to unmask]

Subject: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT



Does anyone have or know where to find the formula for determining the

amount of percentage of gold in a SMT solder joint?  Appreciate any

help, Jon



---------------------------------------------------

Technet Mail List provided a

s a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------







 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2