We need to step, or dispense occasionally, 5% of the time?
If the component that requires less paste is too close to a component that
requires thick paste, a stainless steel blade cannot flex quickly enough to
drop into or pull out of the cavity and produce the desired print thickness.
Since we are a low volume shop, we usually minimize the print and add with
dispensers. In high volume this would be slow.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Friday, December 21, 2012 10:33 AM
To: [log in to unmask]
Subject: [TN] Stepped Stencils
Just a poll to see how many assemblers out there are utilizing stepped
stencils where a thinner stencil is required for ultra fine pitch or 0201 /
1005 components?
How much of your product mix requires a stepped stencil?
What are the draw backs and pitfalls?
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480 x115
F: 607.266.0482
<mailto:[log in to unmask]> [log in to unmask]
P Please consider the environment before printing this e-mail.
_____
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the
property of MPL Incorporated, intended only for the use of the intended
recipient(s). Unauthorized use or disclosure of this information is
prohibited. If you are not an intended recipient, please immediately notify
MPL Incorporated and destroy any copies of this email. Receipt of this
e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or
the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain information
that is company confidential or privileged. Any technical data in this
message may be exported only in accordance with the U.S. International
Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
Administration Regulations (15 CFR Parts 730-774). Unauthorized use is
strictly prohibited and may be unlawful. If you are not the intended
recipient, or the person responsible for delivering to the intended
recipient, you should not read, copy, disclose or otherwise use this
message. If you have received this email in error, please delete it, and
advise the sender immediately.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|