If you have skilled operators, no such procedures are needed, because the 
operator lives with his iron from morning to evening the whole year. He is 
so familiar with his tip (hmm) that he registers every deviation from 
normal.  Sounds like something produced by a green engineer. If you do not 
have skilled operators, then it's better send them on a certification course 
than bother about their tips.

(n the other hand you need calibrate minimum once a year to meet many 
standards.  We use IR meters, faster, better. )

Inge



--------------------------------------------------
From: "Dominic Boudreau" <[log in to unmask]>
Sent: den 18 May 2010 22:06
To: <[log in to unmask]>
Subject: [TN] Solder iron tips calibration

> Hello Technetters, we are presently reviewing our internal procedure for 
> the solder iron calibration. One step of that procedure consists to 
> validate the solder iron tips by measuring the temperature of the tip 
> using a thermometer ( like the Hakko 191). The procedure asks to do the 
> calibration  each week or on each tip substitution for all solder irons.
>
>
>
> I'm not sure where these requirements came, but I would like to know if 
> you think it is necessary to calibrate the solder iron tips (I'm not 
> talking about the calibration of the iron itself) . If yes, what would be 
> the the calibration frequency recommended?
>
>
>
>
>
> Dominic Boudreau, ing.
> Ingénieur de produit / Manufacturing Engineer
> T | 450.967.7100 ext.337
> E | [log in to unmask] <mailto:[log in to unmask]>
> W | www.digico.cc <http://www.digico.cc/>
>
>
> N'imprimer que si nécessaire - Print only if you must
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------  


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2