Sorry, Inge, cannot agree with you on both scores. SnCl2 is soluble in
light alcohols and ketones but insoluble in cyclic solvents. It can
hydrate in water to a dihydrate which is almost insoluble in water at
±pH7 but becomes increasingly soluble at lower pH values and more so at
higher pH values (hence saponifier solutions). It is slightly ionic,
therefore potentially dangerous. I don't know about its hygroscopicity
in its two forms under conformal coating, but I would not instinctively
want it there.
Brian
On 25/08/2011 15:20, Inge Hernefjord wrote:
> Tin Chloride is:
> -insoluble in normal industrial solvents
> -harmless
> /Inge
>
>
>
> On 3 August 2011 19:49, Don McFarland<[log in to unmask]> wrote:
>
>> Any ideas on methods to remove a tin chloride residue that was found on a
>> FR-4 substrate after wave solder. We have done some good homework to find
>> the source, but we are looking for good and proven methods to remove the
>> residues from affected assemblies.
>>
>> Any input is welcome.
>>
>> Regards,
>>
>> Don McFarland
>>
>> **********************************
>> CONFIDENTIALITY NOTICE: The information in this electronic mail
>> transmission is legally privileged and confidential information intended
>> only for the use of the individual or entity named above. If the reader of
>> this message is not the intended recipient, you are hereby notified that any
>> dissemination, distribution or copying of the transmission is strictly
>> prohibited. If you have received this transmission in error, delete the
>> message and immediately notify us by telephone at 435.792.4949 or by
>> responding to this email.
>> **********************************
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> For additional information, or contact Keach Sasamori at [log in to unmask] or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|