We have seen this problem before. Same company, 2 diff assy. locations.
One location specified Dynachem Dry-film to be used on brds supplied to that
facility.
That facility closed down, parts that were left unassembled were transfered
to other facility. Mask started to peel-off.
Solution was, not to throw away the expensive brds....coat it with LPI
soldermask (that was compatible) and use them. It worked.
Rashesh
_www.accueng.com_ (http://www.accueng.com)
818-768-3919
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------