TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 19 Mar 2013 14:28:44 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (110 lines)
Steve,
Let me ask a dumb question - why not just buy a new solder reservoir, save 
yourself the hassle and labor, and sell the whole pot to a reclaimer?

Doug Pauls



From:   Steve Gregory <[log in to unmask]>
To:     <[log in to unmask]>
Date:   03/19/2013 12:11 PM
Subject:        Re: [TN] Solder pot capacity of Vitronics/Soltec 6622CC 
Wave solder machine
Sent by:        TechNet <[log in to unmask]>



Thanks Ed!

I'm learning more & more about this machine as the days tick down, and I 
haven't even seen it yet. To further complicate matters, I understand that 

there's a couple of hundred pounds of what maybe be SAC307 in the bottom 
of 
the pot, was told that it was analysis was this: 96.17 % Tin, .54 % 
copper, 
3.18 % silver. The machine is intended to be used as a 63/37 machine, and 
getting that residual solder out is going to be a bear because I 
understand 
that the bottom of the pot has what's called a "false bottom" or welded 
structure inside, so it's going to be tough. I don't think I can leave the 

solder inside the pot with hopes of adding new solder and it will dilute 
what's left in the pot down enough for the solder to be within spec, in 
fact 
I'm pretty sure it won't, the silver content is especially what worries 
me.

The previous emails from a few days ago about the tin content was with the 

existing wave that they have, now they have the -6622 coming in with this 
issue. Going to have my hands full when I get to Boise, that's for sure...

Steve

-----Original Message----- 
From: Ed Popielarski
Sent: Tuesday, March 19, 2013 12:07 PM
To: [log in to unmask] ; 'Steve Gregory'
Subject: RE: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave 
solder 
machine

Below link says 700Kg = 1543.24. This might be lead-free, so I'd go with 
1800 just to be safe.

http://www.smtnet.com/mart/index.cfm?fuseaction=view_item&item_id=74987


Ed Popielarski
Engineering Manager


                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, March 19, 2013 8:54 AM
To: [log in to unmask]
Subject: [TN] Solder pot capacity of Vitronics/Soltec 6622CC Wave solder 
machine

Hi All!

Does anybody know what the solder pot capacity is of a Vitronics/Soltec 
6622CC wave solder machine is with tin/lead solder in it?

The reason I?m asking is because my new employer bought a used ?6622 and 
needs to know how much solder they should buy to be able to fill the pot. 
They have an old electrovert now that has a 500-lb pot that we?ll be 
using, 
and I told him that wouldn?t be enough to fill the Vitronics machine. I?m 
thinking the 6622 holds around 1,600 ?1,800 lbs., but I?m not sure...

Steve

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________ 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2