RE: [TN] WARPAGEWould that criteria also apply to "populated" boards? I believe he was seeking data for populated boards...curious...would it matter after assembly if they were warped or not???
Franklin
----- Original Message -----
From: Eric Castonguay
To: [log in to unmask]
Sent: Monday, October 28, 2002 10:14 AM
Subject: Re: [TN] WARPAGE
Pankaj,
check in IPC-6012 par. 3.4.4 Bow & Twist. The printed board shall have a maximum bow & twist of 0.75% for boards that use SM components and 1.5% for all other boards. Also, see test method 2.4.22 described in the "IPC-TM-650 test methods manual" on how to measure it.
Eric Castonguay, Eng.
Manufacturing Engineering
www.Hyperchip.com
Montreal, Canada
T. 514 906 2409
F. 514 906 2501
-----Original Message-----
From: Karnwal, Pankaj [mailto:[log in to unmask]]
Sent: Monday, October 28, 2002 02:02
To: [log in to unmask]
Subject: [TN] WARPAGE
> Hi TechNet
>
> Can any body give me the acceptable range of PCB {Populated } For
> Warpage, { Both Throughole And SMD And MIX components} .And how we can
> measure it. Also tell that what IPC states about this.
>
>
> With regards
> Pankaj Karnwal
> Quality Assurance Ext. 211
> BESL A-4,Sec-5 NOIDA , 201301, INDIA
> e mail : <mailto:[log in to unmask]>
> Barco, innovators in image processing
>
>
>
- - - - - - - - DISCLAIMER - - - - - - - -
Unless indicated otherwise, the information contained in this message is
privileged and confidential, and is intended only for the use of the
addressee(s) named above and others who have been specifically authorized to
receive it. If you are not the intended recipient, you are hereby notified
that any dissemination, distribution or copying of this message and/or
attachments is strictly prohibited. The company accepts no liability for any
damage caused by any virus transmitted by this email. Furthermore, the
company does not warrant a proper and complete transmission of this
information, nor does it accept liability for any delays. If you have
received this message in error, please contact the sender and delete the
message. Thank you.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
--------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|