Hi Thomas,
What high rates of temperature change do, is set up transient internal thermal gradients causing differential thermal expansion [on heating] and contraction [on cooling]—and by the way, rapid cooling is worse than rapid heationg, because now you have the solidifying solder involved as well together with the interaction between warping components and PCBs.
Werner
-----Original Message-----
From: Gervascio, Thomas L <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Feb 11, 2011 3:58 pm
Subject: [TN] Wave soldering SMT capacitors
A friend of mine asked a good question, why is that most SMT capacitor specs
call out for a maximum heating rate at SMT of 2-4 C/sec but the same specs allow
a temperature delta at wave soldering of 100-125 C? In case of wave, the time
between preheat and soldering causes a heating rate in excess of the SMT heating
rates. But it is OK to subject the part to the wave solder but not SMT using
those heating and cooling rates?
I never could recall a logical explanation. Called several capacitor
manufacturer's and they seemed to dance around the question.
Any information would be helpful
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|