Hi Folks,
Our company has specified; IPC-SM-840, CLASS T, 0.001-0.002" THICK.
on each board we have had manufactured for the last few years.
I just received notice from our current manufacturer that they cannot
consistently meet this requirement for 1 to 2 thou thickness, and want
to produce a thickness at a minimum of 0.4 thou.
My questions are;
1. Is this standard considered old and I should be looking at specifying
something else?
2. Are there any repercussions in changing to the suggested reduced thickness?
Regards,
Colin Weber
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|