TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 12 Oct 2011 17:14:23 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gregg Owens <[log in to unmask]>
Message-ID:
Subject:
From:
Gregg Owens <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (100 lines)
Phil:

Bees wax may contain organic contaminates which in the right operating environments may cause a contamination issue. That's why it's only a class 3 issue. 

Gregg Owens 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro
Sent: Wednesday, October 12, 2011 4:30 PM
To: [log in to unmask]
Subject: [TN] Lacing tape

I discovered that we are using lacing tape which is wax impregnated to
tie off cabling.  

IPC-A-610 states in section 4.4.1:  "Note: Do not subject wax
impregnated lacing tape to cleaning solvents. Beeswax is unacceptable
for Class 3."

 

I have been asked to find out the reason for this restriction.

 

My immediate answer is that we don't want to take a chance of
re-depositing wax (a contaminant) onto other surfaces that may require
conformal coating or possible onto conductive surfaces such as connector
contacts, switch contacts, etc.

 

Is there another possible reason?

 

We don't expose the lacing tape to solvents, but it is beeswax
impregnated so my recommendation is to have Production go buy the
unwaxed lacing tape that is available.

 

Many lives ago I experimented with making thermoplastic potting
compounds from synthetic polyolefins from Eastman and learned quite a
bit about "wax".   But I don't know the reason why beeswax is prohibited
other than stated above.

 

 

Thanks in advance,

 

Phillip Bavaro

 

 

 


------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2